Advanced casting processes
Lost foam casting (LFC) uses an expendable foam pattern to define the casting, including any gates and runners made as part of the pattern assembly. Each pattern is consumed during the pour, so the moulder does not need to pull it out of the sand before casting.
Patterns are commonly moulded from expanded polystyrene (EPS), expanded PMMA or blends selected for the alloy and casting. Foam sections can be joined into more complex shapes, then assembled into a cluster and connected to the gating system. The assembled pattern takes a refractory coating and is packed in dry, unbonded sand. Sand has to reach and support pockets, recesses and other parts of the pattern that are difficult to fill evenly.
As molten metal advances through the mould, heat decomposes the foam ahead of the advancing metal front. The melt occupies the volume freed by the pattern. The rate at which the pattern breaks down and the ability of the decomposition products to escape influence how smoothly the cavity fills.
Thermal decomposition can produce carbon dioxide, carbon monoxide and organic compounds. The balance of liquid and gaseous products depends on the alloy temperature and the foam. Lower-temperature aluminium casting tends to leave a larger liquid fraction, while much of the decomposition product forms as gas when casting iron or steel.
The refractory coating is a controlled route from the pattern surface into the surrounding sand for decomposition products. Its permeability influences the rate of filling, while its refractory layer helps support the mould surface and keeps the molten metal from directly contacting the loose sand.
In aluminium casting, some liquid products from the first stage of foam decomposition are taken up by the coating. As heating continues, a portion of that material decomposes further into gas, which can pass into the surrounding mould sand. A coating needs both adequate uptake of liquid products and a path for gas to escape.
In iron and steel casting, higher temperatures produce gases earlier. A transient gap can form between the advancing melt and the remaining foam. Gases travel through the coating into the surrounding sand, where some components may condense or undergo further decomposition as the mould heats.
A coating that restricts gas flow can contribute to gas entrapment and porosity. If viscous liquid products pool near the interface, they may block some vent paths or remain ahead of the metal front. Such interruptions in filling can contribute to surface wrinkles, cold shuts and inclusions. Coating performance therefore needs to be assessed alongside the foam, alloy and moulding conditions.
The flask must be compacted evenly before pouring. Uneven packing around undercuts or within a cluster can leave the pattern poorly supported and make venting less predictable. Multiaxis vibration moves sand around the pattern, with the vibration sequence selected for the mould geometry. After cooling, shakeout separates the casting so the sand can be recovered and conditioned for reuse.
| No. | Equipment |
|---|---|
| 1 | Box tilting system |
| 2 | Shakeout with water tube |
| 3 | Vibrating feeder |
| 4 | Bucket elevator |
| 5 | Magnetic separator |
| 6 | Horizontal cooler classifier |
| 7 | Vertical cooler classifier |
| 8 | Sand-feed belt conveyor |
| 9 | Storage hopper |
| 10 | 2D compaction table |
| 11 | 3D compaction table |
| 12 | Casting flask |
| 13 | Vacuum pump and vacuum station |
| 14 | Automatic transfer trolley |
| 15 | Track line |
| 16 | Hydraulic station |
| 17 | Dust extraction system |
| No. | Equipment |
|---|---|
| 1 | Pre-expander with fluid-bed dryer |
| 2 | Storage silo for pattern moulding |
| 3 | Automatic hydraulic EPS shape-moulding machine |
| 4 | Automatic material filling gun, 8-inch stroke |
| 5 | Central vacuum system |
| 6 | Steam boiler |
| 7 | Cooling tower |
| 8 | Accumulator tank, 2 m³ |
| 9 | Hot-wire cutting machine |
| 10 | CNC hot-wire cutting machine |
| 11 | CNC gluing machine for hot and cold adhesive |
| 12 | Coating permeability tester |
| 13 | EPS pentane tester |
| 14 | Pipework set |
| No. | Equipment |
|---|---|
| 1 | Drying-room heating |
| 2 | Slurry mixer |
| 3 | Slurry mixing tank, stainless steel 304 |